Polymer Property : Shear Strength = 4.76 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 4.76 MPa

@Temperature 23.0 °C
690 psi

@Temperature 73.4 °F
Overlap, Polystyrene
3M Scotch-Weld™ TE040 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Shear Strength 4.76 MPa

@Temperature 23.0 °C
690 psi

@Temperature 73.4 °F
Overlap, Polystyrene, Substrate Failure
3M Scotch-Weld™ TE230 Black Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..