Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 30.0 MPa

@Temperature 24.0 °C
4350 psi

@Temperature 75.2 °F
Short Beam
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel
Shear Strength 30.0 MPa

@Temperature 24.0 °C
4350 psi

@Temperature 75.2 °F
Short Beam
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel
Shear Strength 30.0 MPa

@Temperature 22.2 °C
4350 psi

@Temperature 72.0 °F
Lap Shear
Hexcel® Redux® 610W (0.03 psf) Flame retarded epoxy film adhesive
Redux 610 is a modified, flame-retarded epoxy film adhesive curing at 250°F. It is suitable for bonding metal to metal and for sandwich structures where flame retardancy and low heat release are re..
Shear Strength 30.0 MPa

@Temperature 22.2 °C
4350 psi

@Temperature 72.0 °F
Lap Shear
Hexcel® Redux® 610W (0.06 psf) Flame retarded epoxy film adhesive
Redux 610 is a modified, flame-retarded epoxy film adhesive curing at 250°F. It is suitable for bonding metal to metal and for sandwich structures where flame retardancy and low heat release are re..
Shear Strength 30.0 MPa

@Temperature 127 °C
4350 psi

@Temperature 260 °F
Lap Shear
Hexcel® Redux® 641K Modified epoxy film adhesive for bonding metallic and composite components
Redux 641 is a high temperature modified epoxy film adhesive curing at 350°F. It is suitable for bonding metal to metal and for sandwich structures where operating temperatures are experienced up t..
Copyright © lookpolymers.com All Rights Reserved