Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 50.0 MPa @Temperature 80.0 °C |
7250 psi @Temperature 176 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric Fiber: T1000 12K 5H Satin, 283 g/m2Information provided by HexCel |
|||
Shear Strength | 50.0 MPa @Temperature 232 °C |
7250 psi @Temperature 450 °F |
AS4C; Fill Short Beam |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |
|||
Shear Strength | 50.0 MPa @Temperature 23.0 °C |
7250 psi @Temperature 73.4 °F |
Short Beam Shear, Dry; EN2563 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |