Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 54.0 MPa @Temperature 120 °C |
7830 psi @Temperature 248 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric Fiber: T1000 12K 5H Satin, 283 g/m2Information provided by HexCel |
|||
Shear Strength | 54.0 MPa @Temperature 232 °C |
7830 psi @Temperature 450 °F |
T300; Fill Short Beam; AMB |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |
|||
Shear Strength | 54.0 MPa @Temperature 90.0 °C |
7830 psi @Temperature 194 °F |
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre 1947 - 38% resin weight with M46J 52.5% fiber volumeInformation provided by HexCel |