Mechanical Properties Metric English Comments
Shear Strength 60.7 MPa

@Temperature 150 °C
8800 psi

@Temperature 302 °F
ASTM D732
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications. Torlon PAI has the highest..
Shear Strength 60.7 MPa

@Temperature 150 °C
8800 psi

@Temperature 302 °F
ASTM D732
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI)
Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda..
Shear Strength 60.7 MPa

@Temperature 82.2 °C
8800 psi

@Temperature 180 °F
0° Short Beam, Wet
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber
Information provided by HexCel
Shear Strength 60.7 MPa

@Temperature 23.0 °C
8800 psi

@Temperature 73.4 °F
Hexcel® HexPly® F650 Bismaleimide Resin with Graphite F3T584 fabric reinforcement
Aging Data, (T300-3K, 8 H.S.); Laminate Physicals: 59.6% Fiber volume, 34.0% Resin content, 1.0% VoidsInformation provided by HexCel
Shear Strength 60.7 MPa

@Temperature 23.0 °C
8800 psi

@Temperature 73.4 °F
Hexcel® HexPly® F650 Bismaleimide Resin with Quartz 581 fabric reinforcement
Laminate Physicals: 55.4% Fiber volume, 31.4% Resin content, 0.7% Voids, 1.78% gm.cc Specific gravityInformation provided by HexCel