Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 61.4 MPa @Temperature 24.0 °C |
8910 psi @Temperature 75.2 °F |
Short Beam, Skydrol (30 ± 1 days of Type 2 Skydrol Hydraulic Fluid at 140 ± 5°F (60 ± 3°C) |
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |