Polymer Property : Shear Strength = 8910 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 61.4 MPa

@Temperature 24.0 °C
8910 psi

@Temperature 75.2 °F
Short Beam, Skydrol (30 ± 1 days of Type 2 Skydrol Hydraulic Fluid at 140 ± 5°F (60 ± 3°C)
Hexcel® HexPly® F522 Epoxy Resin, W3C282 Carbon Fabric
Hexcel designation: TW3C282-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel