Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 43.0 MPa @Temperature 140 °C |
6240 psi @Temperature 284 °F |
ILSS; prEN2563 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric Fiber: T1000 12K 5H Satin, 283 g/m2Information provided by HexCel |
|||
Shear Strength | 43.0 MPa @Temperature 90.0 °C |
6240 psi @Temperature 194 °F |
0°, Interlaminar, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, HTA Fiber Designation: C193PW, Plain weaveInformation provided by HexCel |
|||
Shear Strength | 43.0 MPa @Temperature 23.0 °C |
6240 psi @Temperature 73.4 °F |
Lap Shear; Cured 5 days at 23°C; Substrate: 2024 T3 Aluminum Alloy; EN2243-1 |
Hexcel® Redux® 870 A/B Two Component Shimming and Potting Epoxy Paste Adhesive Redux 870 A/B is a two component high performance epoxy paste adhesive, ideal for use as a Liquid Shim or for potting applications. This high temperature performing thixotropic adhesive has been spe.. |
|||
Shear Strength | 43.0 MPa @Temperature 180 °C |
6240 psi @Temperature 356 °F |
Short Beam Shear, Dry; EN2563 |
Hexcel® HexTOOL™ M61 Quasi-isotropic High Temperature Prepreg Tooling Compound HexTOOL™ Tooling Compound is randomly layered strips of uni-directional prepreg which is consolidated into rolled goods. It can be utilized as multi-ply quasi-isotropic hand lay-up, and subsequentl.. |