Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 68.0 MPa @Temperature 177 °C |
9860 psi @Temperature 351 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel |
|||
Shear Strength | 68.0 MPa @Temperature 23.0 °C |
9860 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |