Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 68.0 MPa

@Temperature 177 °C
9860 psi

@Temperature 351 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape
Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel
Shear Strength 68.0 MPa

@Temperature 23.0 °C
9860 psi

@Temperature 73.4 °F
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form
Fibers: T300-3K, AS4C-3KInformation provided by HexCel