Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.0483 MPa @Temperature 110 °C, Time 605000 sec |
7.00 psi @Temperature 230 °F, Time 168 hour |
Overlap |
3M Weatherban™ 5354 Sealant Tape 3M™ Weatherban™ Sealant Tape 5354 is a high tack extruded synthetic rubber, non-curing sealant in tape form.It can be used to seal between glass, metal, wood and many plastics.Easy to compress and.. |
|||
Shear Strength | 0.0483 MPa @Time 86400 sec |
7.00 psi @Time 24.0 hour |
Overlap |
3M Weatherban™ 5354 Sealant Tape 3M™ Weatherban™ Sealant Tape 5354 is a high tack extruded synthetic rubber, non-curing sealant in tape form.It can be used to seal between glass, metal, wood and many plastics.Easy to compress and.. |