Mechanical Properties Metric English Comments
Shear Modulus 1.292 GPa

@Temperature 170 °C
187.4 ksi

@Temperature 338 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..