Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Modulus | 1.473 GPa @Temperature 130 °C |
213.6 ksi @Temperature 266 °F |
DAM; Dynamic; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |