Polymer Property : Shear Modulus = 3480 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 24.0 GPa

@Temperature 300 °C
3480 ksi

@Temperature 572 °F
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F
Information provided by PEAK Werkstoff GmbH
Shear Modulus 24.0 GPa

@Temperature 200 °C
3480 ksi

@Temperature 392 °F
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Shear Modulus 24.0 GPa

@Temperature 250 °C
3480 ksi

@Temperature 482 °F
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Shear Modulus 24.0 GPa

@Temperature 300 °C
3480 ksi

@Temperature 572 °F
PEAK Werkstoff DISPAL S541 Aluminum Alloy, AlMg6Mn4SiTiZr, Condition F
Information provided by PEAK Werkstoff GmbH
Shear Modulus 24.0 GPa

@Temperature 200 °C
3480 ksi

@Temperature 392 °F
Condition T6
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4
High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH
Shear Modulus 24.0 GPa

@Temperature 250 °C
3480 ksi

@Temperature 482 °F
Condition T6
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4
High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH