Polymer Property : Shear Modulus = 506.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Modulus 3.494 GPa

@Temperature -20.0 °C
506.8 ksi

@Temperature -4.00 °F
DAM; Dynamic; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G30HSLR BK099 Nylon 66  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G30HSLR BK099 is a 30% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..