Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 96.0 - 111 °C | 205 - 232 °F | Average value: 104 °C Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |