Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 96.0 °C @Load 1.00 kg |
205 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexi.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Rate A; ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® PS 1328 PRE-ELEC PS 1328 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CY6120 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS featuring good flow and impact properties. UL-94 V0 listed at 1.2mm intended for various thin wall applications. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® EX58 ABS High impact ABS for sheet extrusion and blow molding applications. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Rate B; ASTM D1525 |
Ineos Nova FX550 (ASTM) Advanced Styrenic Polymer
(discontinued **) Extremely high glossHigh Izod impact strengthUL Classification 94 HBPractical toughnessHigh flow for injection moldingScuff resistanceApplications: Replacement resin for selected ABS applicationsRef.. |
|||
Vicat Softening Point | 96.0 - 111 °C | 205 - 232 °F | Average value: 104 °C Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D1525 |
Huntsman PE1020 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Medium impact strength and good processability.Applications: Film extrusion: general purpose packaging.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 .. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D1525 |
Huntsman PE1055 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D1525/A |
Gichem GILAC E200 Acrylonitrile Butadiene Styrene
(discontinued **) ABS medium fluidity, excellent resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D1525 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 16% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | 1 kg; ASTM D1525 |
LG Chemical HI855M PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D1525 |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical RS657L ABS, Chemical Resistance to Cyclopentane, Low Specific Gravity Feature: Extrusion Molding, Chemical Resistance to Cyclopentane, Thin ThicknessApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical RS800M ABS, High Modulus, Chemical Resistance to HCFC Feature: Extrusion Molding, High Modulus, Chemical Resistance to HCFCApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D1525 |
Hannam Chemical Hanalac 711 ABS, Plating Grade Plating grade with excellent moldability and easy to surface treat. It also has a strong adhesive strength after plating and an excellent heat cycle. Applications: Appliances, TV frames, automoti.. |
|||
Vicat Softening Point | 96.0 °C @Load 5.00 kg |
205 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical GPPS 25SP(I) PS, High Transparency, Heat Resistance Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical |
|||
Vicat Softening Point | 96.0 °C | 205 °F | |
Ineos Styrenics Polystyrene 145D (NAFTA) A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics pu.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Xylex X8300HP PC+POLYESTER (Europe-Africa-Middle East) Transparent, US Food Contact compliant, chemically resistant.
This grade will no longer be supported with biocompatibility information and should not be used for medical applications which require b.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Unannealed; ISO R 306 |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Vicat Softening Point | 96.0 °C @Load 5.10 kg |
205 °F @Load 11.2 lb |
120°C/h; ASTM D 1525 |
Styrolution Absolac® 100 ABS Super high impact gradeMedium flowInformation provided by Styrolution |
|||
Vicat Softening Point | 96.0 °C | 205 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SC 201LV General Purpose Polystyrene CharacteristicsHigh molecular weight grade Good flow properties along with good mechanical strength Easy process ability with good mold release propertiesProcessing Injection moldingApplicationsSuit.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | 1kg / 120°C; ASTM D1525 |
Supreme Petrochem SP6489 9940 High Impact Polystyrene Characteristics High flow Good toughness Available in black only Processing Injection moldingApplications TV and audio-video back and front cover Material Status: Commercial : ActiveAgency Ratings.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS high gloss Noryl |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | Conditioned 4 hours @ 70°C (158°F); ASTM D1525 |
Eastman Tenite Propionate 307A2R30013 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D-1525 |
Chevron Phillips MarFlex® 1125 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for blown film applications that require: Good impactNo slip, includes antiblockGood processabilityGood sealabilityGood drawdown Applications: Typi.. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | ASTM D1525 |
Diamond Polymers MS-170 Styrene Methyl Methacrylate Terpolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 96.0 °C | 205 °F | 50°C/hr; 50N |
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion.. |