Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Riblene® MR 10 Low Density Polyethylene - Injection Molding Riblene MR 10 is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 are characterized by a high flexibility.Main Applications: Riblene MR 10 is suitable for injecti.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycolac® FR15 ABS Flame retardant ABS (non-PBBE additive). Good property/toughness. Excellent moldability. UL94 V-0/5VA rated. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306/B50 |
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b.. |
|||
Vicat Softening Point | 83.9 °C | 183 °F | ASTM D1525 |
ExxonMobil Escorene® LD 712.06 Film Resin
(discontinued **) Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
Covestro Bayblend® R-FR 390 Polycarbonate/ABS Blend
(discontinued **) FR-recycled grades with variable recycled content.Applications: Housings for office equipment, electrical engineering, computer sectors.Information provided by Bayer.As of 1 September 2015, Bayer Ma.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
Eastman Tenite 131E-28 Cellulose Acetate
(discontinued **) 28% plasticized and contains 50% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
LyondellBasell Petrothene® NA204000 Low Density Polyethylene ApplicationsPETROTHENE NA 204-000 is a general-purpose resin recommended for intermediate and light-weight coating applications at high speeds. NA 204-000 can be drawn down to weights of 2.0 lb/rea.. |
|||
Vicat Softening Point | 84.0 °C @Load 5.00 kg |
183 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
LG Chemical AF312T ABS, Flame Retardant Feature: Injection Molding, Flame RetardantApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 79-94-7 and 1309-64-4Information provided by LG Chemical.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306 |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306A |
Lucite International Elvakon® 4490 High Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable pr.. |
|||
Vicat Softening Point | 83.9 °C | 183 °F | Phr = 8 |
Shandong Rike Chemical HELIâ„¢ HL-56 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | VST/B/50; ISO 306 |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | VST/B/50; ISO 306 |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 175A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® NH-1926 HIPS, Unreinforced FR Non-halogen flame-retardant HIPS with high-impact that can be used in the exterior of TV and VCR interior/exterior material of OA devicesInformation provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 83.9 °C | 183 °F | 120°C/hr, 10N; ASTM D1525 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ISO 306 |
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1700 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade for easy flow injection molding of flexible parts, powder production for grindin.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total PSI 8350 High Impact Polystyrene 8350 is a very high impact polystyrene for extrusion. This grade has an improved environmental stress crack resistance in comparison with standard high impact grades. It is proposed for the produc.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | ASTM D1525 |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Vicat Softening Point | 84.0 °C @Load 1.00 kg |
183 °F @Load 2.20 lb |
ASTM D1525 |
Eastman Eastar DN001HF Copolyester Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to p.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
Covestro Bayblend® FR 86 Polycarbonate/ABS Blend Easy-flowing FR grade. Flame retardant grade with antimony, chlorine and bromine free, flame retardant package.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separat.. |
|||
Vicat Softening Point | 83.9 °C | 183 °F | ASTM D1525 |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N; ISO 306 |
Denka TH-11 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50N; ISO 306 |
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
BASF Polystyrol® 144 C Polystyrene (Europe) Very easy flowing grade, often blended with impact-modified Polystyrol or used as a coextruded glossy layer.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | |
BASF Polystyrol® 143 EO Polystyrene (Europe) Easy flowing grade for the injection molding and extrusion of low-taint food packaging.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 83.9 °C | 183 °F | ASTM D1525 |
Global S-1018 Low Density Polyethylene, Injection Molding Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-packagingMeets FDA requirements as listed in food additives regulation 21 CFR 117.15.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/hr; 50N |
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade
(discontinued **) OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall.. |
|||
Vicat Softening Point | 84.0 °C | 183 °F | 50°C/h; 50N; 10x10x4mm; ISO 306/B50 |
SYNTHOS Krasten® 552M High Impact Polystyrene High impact grade with a wide range of Applications. Processed mainly by injection moulding. Production of consumer goods and technical parts subjected to increased mechanical stress. Good results i.. |