Material Notes:
Applications:DisplaysPersonal care and CosmeticsProduct Description: Eastar Copolyester DN001HF has excellent flow characteristics while maintaining superior mechanical properties. It is easy to process and can fill intricate tools. Its most outstanding features are clarity, toughness and chemical resistance. This product has been GREENGUARD INDOOR AIR QUALITY CERTIFIED®.Information provided by Eastman.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Water Absorption 0.15 %

@Time 86400 sec
0.15 %

@Time 24.0 hour
Immersion; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength at Break 38.0 MPa
5510 psi
ASTM D638
Tensile Strength, Yield 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 260 %
260 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 0.690 J/cm

@Temperature -40.0 °C
1.29 ft-lb/in

@Temperature -40.0 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Izod Impact, Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D4812
NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
ASTM D4812
Puncture Energy 46.0 J

@Temperature -40.0 °C
33.9 ft-lb

@Temperature -40.0 °F
At Max load; ASTM D3763
47.0 J

@Temperature 23.0 °C
34.7 ft-lb

@Temperature 73.4 °F
At Max load; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C
153 °F
ASTM D648
Vicat Softening Point 84.0 °C

@Load 1.00 kg
183 °F

@Load 2.20 lb
ASTM D1525
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
Total; ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 250 - 270 °C
482 - 518 °F
Mold Temperature 15.0 - 30.0 °C
59.0 - 86.0 °F
Drying Temperature 71.0 °C
160 °F
Dry Time 6 hour
6 hour