Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 80.0 - 112 °C | 176 - 234 °F | Average value: 95.1 °C Grade Count:13 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |