Polymer Property : Vicat Softening Point = 257 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 257 °C
495 °F
49 N; ISO 306, ASTM D1525
Nilit Nilamid A G7 FR PH1 35% Glass Fiber Reinforced, Flame Retardant PA66 (with Red Phosphorous)
Description: Nilamid A G7 FR PH1 combines flame retardancy with outstanding mechanical performance. This product has a UL 94 V0 listing 1.5 and a complete yellow card. The formulation has been optim..
Vicat Softening Point 257 °C
495 °F
49 N; ISO 306, ASTM D1525
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66
Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,..
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1006 TPI Blend
High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha..
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1006M TPI Blend
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1016 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant, High Flow
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant, High Flow
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Extem UH1016M TPI Blend
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 257 °C
495 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 257 °C
495 °F
9.8 N; ISO 306, ASTM D1525
Nilit Nilamid A3 H G7 General Purpose 35% Glass Reinforced PA66
Description: Nilamid A3 H G7 is a general purpose 35% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
Vicat Softening Point 257 °C
495 °F
9.8 N; ASTM D1525
Nilit Polynil® P50FL Externally Lubricated, Lightly Nucleated Nylon 66
Description: Polynil P50FL is a general purpose injection molding grade that is widely used for gears, bearings, fasteners, clips.Key characteristics: Excellent flowGood toughnessGood overall mechan..
Vicat Softening Point 257 °C
495 °F
DAM; 50°C/h 50N; ISO 306
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66  (Unverified Data**)
Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high producti..
Vicat Softening Point 257 °C
495 °F
B/120; ISO 306
Eurostar Starflam AFR560B5 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR560B5 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Vicat Softening Point 257 °C
495 °F
DAM; 50°C/h 50N; ISO 306
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol..