Polymer Property : Vicat Softening Point = 274 °F
Polymer Property :
Vicat Softening Point =
274 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Vicat Softening Point
134
°C
274
°F
Rate A; ASTM D1526
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester