Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 134 °C | 273 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200 is a PC+ABS blend developed to serve extremely demanding applications in a variety of markets while maintaining good processing properties. The combination of superior heat resistance .. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East) C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific) Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 134 °C @Load 5.001 kg |
273 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB SCANBLEND FS8 PC/ASA, Improved Weather Resistance Information provided by Polykemi AB |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® FXE4472L PC (Asia Pacific) Lexan* FXE4472L is a 20% glass filled, impact modified polycarbonate with excellent light-shield capability. It is designed for high flow, superior surface appearance, enhance release and good impac.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1200HF is the improved version of CYCOLOY C1200 and has been developed to provide enhanced productivity and surface appearance for |
|||
Vicat Softening Point | 134 °C @Load 1.00 kg |
273 °F @Load 2.20 lb |
ASTM D1525 |
LG Chemical SEETEC R3420 Polypropylene, Random Copolymer Features: Seetec R3420 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance.. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
Vicat Softening Point | 134 °C | 273 °F | VST/A/50; ISO 306 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Vicat Softening Point | 134 °C | 273 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 134 °C | 273 °F | B/50; ISO R306 |
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 134 °C | 273 °F | 50°C/h 50N; ISO 306 |
Covestro Bayblend® KU 2-1514* Polycarbonate + ABS, Flame Retardant Grade Developmental productHigh heat resistant injection molding gradeball indentation temperature =125 °CVicat/B 120 temperature = 136 °CUL-listing 94 V-0 at 1.5 mmsuitable for supporting life componen.. |
|||
Vicat Softening Point | 134 °C @Load 5.10 kg |
273 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® ET UV120 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent.. |
|||
Vicat Softening Point | 134 °C @Load 1.00 kg, Thickness 3.17 mm |
273 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1525 |
Diamond Polymers ABS 4107 Heat Resistant Grade Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Vicat Softening Point | 134 °C | 274 °F | Rate A; ASTM D1526 |
Clariant Renol TPU1088A Polyurethane Elastomer, Aromatic Polyester Data provided by Clariant Masterbatches |
|||
Vicat Softening Point | 134 °C | 273 °F | |
Covestro Bayblend® KU 2-1468 Polycarbonate/ABS Blend Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Vicat Softening Point | 134 °C @Load 5.10 kg |
273 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® ET UV130 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent.. |
|||
Vicat Softening Point | 134 °C | 273 °F | 50°C/hr; 50N |
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Vicat Softening Point | 134 °C | 273 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only. |