Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 505R PC (Asia Pacific) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 505RU PC (Asia Pacific) Lexan* 505RU is a glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEEE/Ro.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® 505RU PC (Europe-Africa-Middle East) Lexan* 505RU is a 10% glass reinforced,flame retardant(FR)grade with non brominated and non chlorinated FR systems and UV stablization packages. This product is intended for applications to meet WEE.. |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/h |
Radici Heraflex® E 4718 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. Low Modulus, Nominal Shore D/15s 43. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® BFL2015 PC Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FR2-D Polycarbonate, Improved Flame Retardant, Medium Flow Polycarbonate, Improved Flame Retardant, Medium FlowFeatures: • High Impact Resistance • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® PK2870 PC (Europe-Africa-Middle East) LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas region. |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FR1-D-[color]-3 Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilized Polycarbonate, Improved Flame Retardant, Low Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples... |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-FR3A-D-[color]-3 Polycarbonate, Flame Retardant, High Flow, UV-stabilized Polycarbonate, Flame Retardant, High Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informat.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 120°C/h, 50 N; ASTM D1525 |
Polymer Resources PC-UV3-D-[color]-1 Polycarbonate, UV-stabilized, High Flow with Mold Release Polycarbonate, UV-stabilized, High Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1302-10 Polycarbonate Resin Description: LUPOY PC 1302-10 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength... |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/hr; ASTM D1525 |
LG Chemical Lupoy 1303AH-10 Polycarbonate Resin Description: LUPOY PC 1303AH-10 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and .. |
|||
Vicat Softening Point | 149 °C | 300 °F | ISO 306/B50 |
Styron CALIBREâ„¢ 200-10 Polycarbonate Resin Overview: CALIBREâ„¢ 200-10 Series are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance, heat distor.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N Load; ASTM D1525 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N; ASTM D1525 |
Styron EMERGEâ„¢ 4330-10 Polycarbonate EMERGEâ„¢ PC 4330-10 advanced resin is a polycarbonate resin offering ultraviolet light stability, high heat resistance and maximum toughness. Applications: Consumer Electronics and Information.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific) PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump .. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate A (50°C/h); ASTM D1525; ISO 360/B50 |
Styron CALIBREâ„¢ 300-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 a.. |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® LV-2250Y Standard (mold release/ice color grade) Polycarbonate Resin Flame retardant and mold release grade, while maintaining intrinsic transparency of polycarbonate resin. It is suitable for injection molding applications, required for normal fluidity.Applications:.. |
|||
Vicat Softening Point | 149 °C | 300 °F | |
Covestro Makrolon® 8035 Polycarbonate High viscosity extrusion and injection molding grade with 30% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b.. |
|||
Vicat Softening Point | 149 °C | 300 °F | |
Covestro Makrolon® 8345 Polycarbonate High viscosity injection molding and extrusion grade with 35% standard glass fibers and easy mold release, stiff flow, especially high strength and stiffness.Information provided by Bayer.As of 1 Se.. |
|||
Vicat Softening Point | 149 °C | 300 °F | ISO 306/A50 |
ExxonMobil PP7011L1 Polypropylene Impact Copolymer Product Description: An impact copolymer resin for extrusion applications with high melt viscosity and excellent low-temperature impact strength. It is suitable for cables, pipes, profiles, sheets .. |
|||
Vicat Softening Point | 149 °C | 300 °F | -1kg; ASTM D1525 |
Braskem H 604 Blow Molding Polypropylene Applications: Transparent bottles for mineral water, cosmetic, health care and cleaning products. Information provided by Braskem |
|||
Vicat Softening Point | 149 °C | 300 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® GV-3410R High Flame Retardancy, Glass Fiber Reinforced Polycarbonate Resin GF 10% reinforced, improved flame retardance and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecis.. |
|||
Vicat Softening Point | 149 °C | 300 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Noryl GFN1430V PPE+PS (Europe-Africa-Middle East) Noryl* GFN1430V PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability. This grade has been developed for potable.. |
|||
Vicat Softening Point | 149 °C | 300 °F | -1kg; ASTM D1525 |
Braskem H 152 Fiber Extrusion Polypropylene Applications: Nonwoven by blow process for disposable diapers, personal care and disposable medical care. Information provided by Braskem |