Vicat Softening Point 198 °C
388 °F
ASTM D1525
Multibase Nylex™ 4650 Polyamide + PP
Mineral filler, 33% Filler by WeightForms: PelletsInformation provided by Multibase
Vicat Softening Point 198 °C
388 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66
Conductive GTX, CTE 7
Vicat Softening Point 198 °C
388 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific)
Conductive GTX, CTE 7
Vicat Softening Point 198 °C
388 °F
Rate B/50; ISO 306
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 7
Vicat Softening Point 198 °C
388 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Vicat Softening Point 198 °C
388 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Asia Pacific)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Vicat Softening Point 198 °C
388 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
Vicat Softening Point 198 °C
388 °F
Rate B/120; ISO 306
SABIC Innovative Plastics NORYL GTX GTX673 PPE+PA
Conductive Noryl GTX* resin designed for profile extrusion. This grade can be electrostatic or powder coat painted without the need for a primer. In addition, its high heat capability allows it to ..
Vicat Softening Point 198 °C
388 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Vicat Softening Point 198 °C
388 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Asia Pacific)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Vicat Softening Point 198 °C
388 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Vicat Softening Point 198 °C
388 °F
10 N - A method; ISO 306
Arkema Group Orgalloy® LT 5050 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
Vicat Softening Point 198 °C
388 °F
10 N - A method; ISO 306
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group