Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 43.9 °C | 111 °F | ASTM D1525 |
ExxonMobil Escorene® LD 767.MJ Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |