Polymer Property : Vicat Softening Point = 502 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 261 °C
502 °F
B
Plastcom SLOVAMID 66 GF 13 TS PA66, 13% glass fibre
FeaturesChemically reinforced with 13% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W..
Vicat Softening Point 261 °C
502 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1016 TPI Blend
High heat amorphous TPI Blend, Chemical Resistant, High Flow
Vicat Softening Point 261 °C
502 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical Resistant, High Flow
Vicat Softening Point 261 °C
502 °F
Rate B/50; ISO 306
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical Resistant, High Flow
Vicat Softening Point 261 °C
502 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Extem UH1016M TPI Blend
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Americas region.
Vicat Softening Point 261 °C
502 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Extem UH1016M TPI Blend (Asia Pacific)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 261 °C
502 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Extem UH1016M TPI Blend (Europe-Africa-Middle East)
High heat amorphous TPI Blend, Chemical ResistantThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.