Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 57.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 57.0 °C
135 °F
Vicat A, 1 kg; DIN 53460/ISO 306
Advanced Elastomer Systems VistaFlex® 911-N Thermoplastic Rubber  (discontinued **)
Description: A colorable high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as fr..
Vicat Softening Point 57.0 °C
135 °F
ASTM D1525
DuPont Bynel® 2014 Acid-Modified Ethylene Terpolymer Adhesive Resin  (discontinued **)
Bynel® Series 2000 resins are acid-modified ethylene terpolymers with medium to high acid comonomer contents. They contain a temperature stable ester that makes them functional in high-temperature ..
Vicat Softening Point 57.0 °C
135 °F
ASTM D1525
DuPont Bynel® 3120 Acid-/Acrylate-Modified EVA Adhesive Resin  (discontinued **)
Bynel® Series 3100 resins are acid/acrylate-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to proce..
Vicat Softening Point 57.0 °C
135 °F
1000g; ASTM D-1525
ExxonMobil Escorene® LD-722 High EVA Film and Compounding Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr..
Vicat Softening Point 57.0 °C
135 °F
Rate B; ASTM D-1525
ExxonMobil Iotek® 8610 Sodium Ionomer  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A low melt index sodium ionomer made from an ethylene acrylic acid base polymer. It is designed to have high durability, resilience and impact stre..
Vicat Softening Point 57.0 °C
135 °F
Eastman Ecdel PCCE 9966 Copolyester Ether Elastomer
ISO data as provided by the manufacturer, Eastman Chemical
Vicat Softening Point 57.0 °C
135 °F
ASTM D1525, ISO 306
DuPont™ Bynel® 21E810 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester that allows them to be functional in high temperature coextrusions. They are avail..
Vicat Softening Point 57.0 °C
135 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
Vicat Softening Point 57.0 °C
135 °F
Rate B, ASTM D1525-70
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc
Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi..
Vicat Softening Point 57.0 °C
135 °F
BASF Novolen® 2500 MC Polypropylene
Data was collected by ISO methods and provided by BASF.
Vicat Softening Point 57.0 °C
135 °F
Biomer P209 PHB Biodegradable Polymer
PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P..
Vicat Softening Point 57.0 °C
135 °F
A50; ISO 306
Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade)
Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible..