Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58238 Ester Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimInformation provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 75
75
ISO 868
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ISO 37
Elongation at Break 730 %
730 %
ISO 37
Tensile Modulus 0.0100 GPa
1.45 ksi
ISO 527
50% Modulus 0.00260 GPa
0.377 ksi
ISO 37
100% Modulus 0.00310 GPa
0.450 ksi
ISO 37
300% Modulus 0.00450 GPa
0.653 ksi
ISO 37
Rebound 56 %
56 %
ISO 4662
Tear Strength 45.0 kN/m
257 pli
with incision; ISO 34B
53.0 kN/m
302 pli
without incision; ISO 34B
Abrasion 40
40
mm<sup>3</sup>; ISO 4649
Compression Set 31 %
31 %
70 hrs./22°C; ISO 815
73 %
73 %
24 hrs./70°C; ISO 815
Thermal Properties Metric English Comments
Vicat Softening Point 57.0 °C
135 °F
A50; ISO 306
Users viewing this material also viewed the following: