Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 57.2 °C | 135 °F | VST/A/50; ISO 306 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D1525 |
ExxonMobil Escor™ 5200 Ethylene Acrylic Acid Copolymer Resin Product Description: Escor 5200 is an ethylene acrylic acid copolymer with a high comonomer content. Escore 5200 can be used pure or as a component in blend formulations for bonding applications whe.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D882 |
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D1525 |
Dow AMPLIFY™ EA 101 Ethylene-ethyl Acrylate (EEA) AMPLIFY™ EA 101 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility and imparts low temperature toughness to a wide range of engineering resins. This polymer.. |
|||
Vicat Softening Point | 57.2 °C | 135 °F | ASTM D882 |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |