Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 300 °C | 572 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Vicat Softening Point | 300 °C | 572 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7301 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Vicat Softening Point | 300 °C | 572 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 50 PEEK Polyetheretherketone (PEEK). Unfilled. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; Asia Pacific; Europe;.. |
|||
Vicat Softening Point | 300 °C | 572 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Vicat Softening Point | 300 °C | 572 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105/CF/10/GR/10/TF/10-2 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Vicat Softening Point | 300 °C | 572 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-0831 PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Vicat Softening Point | 300 °C | 572 °F | DIN ISO 306 |
Lehmann & Voss LUVOCOM® 1105-7685 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Super.. |
|||
Vicat Softening Point | 300 °C | 572 °F | VST/B/50; ISO 306 |
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber Polyether etherketone can be used at very high temperatures and it shows a good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical .. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Laticonther 88/10 GR/50 PEEK, 50% Graphite Reinforced High thermal conductivity product based on Polyetheretherketone (PEEK). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Latigray 88/10-01 CX/30 PEEK Radiopaque compound based on Polyetheretherketone (PEEK). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Vicat Softening Point | >= 300 °C @Load 5.00 kg |
>= 572 °F @Load 11.0 lb |
|
LATI Latiohm 88/10-06 CNT PEEK Semiconductive/dissipative product based on Polyetheretherketone (PEEK). Carbon nanotubes. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |