Polymer Property : Vicat Softening Point = 58.3 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 58.3 - 119 °C
137 - 246 °F
Average value: 100 °C Grade Count:231
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Vicat Softening Point 58.3 °C
137 °F
50°C/hr; 50N; ASTM D1525
Arkema Group Solarkote® P-610 Acrylic
PVC Capstock, clear, low glossInformation provided by Arkema Group
Vicat Softening Point 58.3 °C
137 °F
50°C/hr; 50N; ASTM D1525
Arkema Group Solarkote® P-600 Acrylic
PVC Capstock, clear, high glossInformation provided by Arkema Group
Vicat Softening Point 58.3 °C
137 °F
50°C/hr; 50N; ASTM D1525
Arkema Group Solarkote® P-601 Acrylic
PVC Capstock, white, high glossInformation provided by Arkema Group
Vicat Softening Point 58.3 °C
137 °F
50°C/hr; 50N; ASTM D1525
Arkema Group Solarkote® P-611 Acrylic
PVC capstock, white, low glossInformation provided by Arkema Group