Thermal Properties Metric English Comments
Vicat Softening Point 58.3 - 119 °C
137 - 246 °F
Average value: 100 °C Grade Count:231
Overview of materials for Acrylic, General Purpose, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values ..
Vicat Softening Point 95.0 - 119 °C
203 - 246 °F
Average value: 105 °C Grade Count:13
Overview of materials for Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE)/Hexene, Film Grade". Each property range of values reported is m..