Polymer Property : Vicat Softening Point = 617 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7192 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7460/BL5019 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Chemical and hydrolysis resistance parts, non flamm..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-8355 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-8513 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Vicat Softening Point >= 325 °C
>= 617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/CF/30/EM PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/RD PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/GF/30/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/GN7348 PEEK, unreinforced, laser markable
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Not flammable.Especially suitable for medica..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-0904/GN PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-0918/EM/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7310 PEEK, with glass fiber, easy flowing, low-warpage
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High dimensionally stable precision parts, high continuous use temperature.Superheated ste..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105/GF/40 PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Vicat Softening Point 325 °C
617 °F
DIN ISO 306
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa..