Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 40.0 - 80.0 °C | 104 - 176 °F | Average value: 56.9 °C Grade Count:22 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RH 211/W Rigid PVC, Antishock Extrusion Various antishock profiles |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RH 212/W Rigid PVC, Antishock Extrusion Outdoor antishock profiles |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 115 Rigid PVC, Extrusion Lead Free Small tubes for shoes |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 317/UV Rigid PVC, Extrusion Lead Free Profiles anti-UV |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 212/W Rigid PVC, Antishock Extrusion Lead Free Outdoor antishock profiles |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 311 Rigid PVC, Antishock Extrusion Lead Free Antishock profiles |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 315/W Rigid PVC, Antishock Extrusion Lead Free Various profiles antishock |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock UV resistant |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 116 Rigid PVC, Extrusion Small tubes for shoes |
|||
Vicat Softening Point | 70.0 - 80.0 °C | 158 - 176 °F | Average value: 76.7 °C Grade Count:3 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |