Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 80.6 °C | 177 °F | ASTM D1525 |
ExxonMobil Escorene® LD 319.92 Film Resin
(discontinued **) Escorene Ultra LD 319.92 is a 9.0 wt% vinyl acetate copolymer film resin, that exhibits superior impact strength and heat sealability.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 80.6 °C @Load 0.999 kg |
177 °F @Load 2.20 lb |
120°C/hr, 9.8N; ASTM D1525 |
Lubrizol Estane® 2355-95AEF Thermoplastic Polyurethane Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation |
|||
Vicat Softening Point | 80.6 °C | 177 °F | ASTM D-1525 |
Chevron Phillips K-Resin® KR03BR SBC
(discontinued **) K-Resin® Styrene-Butadiene Copolymer (SBC)Applications:BottlesMolded boxes and containersMedical devicesPortion packagesBlister packagingFeatures:Good stiffnessGood formabilityGood toughnessExcelle.. |