Material Notes:
Type: Pellethane® 2355-95AEF is a thermoplastic polyurethane elastomer.Feature: Film resin, Fuel resistant, Blow molding grade resin.Information Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0090 cm/cm
0.0050 - 0.0090 in/in
Transverse direction; ASTM D955
0.0060 - 0.0090 cm/cm
0.0060 - 0.0090 in/in
Flow direction; ASTM D955
Melt Flow 13 g/10 min

@Load 8.70 kg,
Temperature 190 °C
13 g/10 min

@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ASTM D2240
Tensile Strength, Ultimate 38.9 MPa
5640 psi
ASTM D412
Elongation at Break 450 %
450 %
ASTM D412
50% Modulus 0.00830 GPa
1.20 ksi
ASTM D412
100% Modulus 0.00970 GPa
1.41 ksi
ASTM D412
300% Modulus 0.0214 GPa
3.10 ksi
ASTM D412
Flexural Modulus 0.0896 GPa
13.0 ksi
ASTM D790
Tear Strength 105 kN/m
599 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 4.0
4.0
H-22 (coarser); ASTM D1044
Compression Set 30 %

@Temperature 25.0 °C,
Time 79200 sec
30 %

@Temperature 77.0 °F,
Time 22.0 hour
Method B; ASTM D395
80 %

@Temperature 70.0 °C,
Time 79200 sec
80 %

@Temperature 158 °F,
Time 22.0 hour
Method B; ASTM D395
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 153 µm/m-°C
85.0 µin/in-°F
ASTM D696
Vicat Softening Point 80.6 °C

@Load 0.999 kg
177 °F

@Load 2.20 lb
120°C/hr, 9.8N; ASTM D1525
Glass Transition Temp, Tg -15.0 °C
5.00 °F
DSC
Processing Properties Metric English Comments
Melt Temperature 182 - 199 °C
360 - 390 °F
Extrusion
Mold Temperature 16.0 - 60.0 °C
60.8 - 140 °F
Drying Temperature 88.0 - 104 °C
190 - 219 °F
Air dew point <-40°C
Descriptive Properties Value Comments
Elongation Set After Break (%) 60
ASTM D412