Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 83.8 °C | 183 °F | Phr = 8 |
Shandong Rike Chemical HELIâ„¢ HL-35 Weather-resistance Acrylic Impact Modifier (AIM) Outline of ACR Impact Modifiers:The PVC impact modifiers developed by our company are acrylic copolymers (ACR) with a core-shell structure, their cores are acrylic ester and shells are methacrylic c.. |