Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 52.0 - 87.0 °C | 126 - 189 °F | Average value: 80.0 °C Grade Count:123 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Vicat Softening Point | 85.0 - 87.0 °C @Load 5.00 kg |
185 - 189 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 244 Rigid PVC, Extrusion Shutters high modulus low curving |