Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 48.0 - 90.0 °C | 118 - 194 °F | Average value: 74.4 °C Grade Count:12 |
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum an.. |