Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade

Category Polymer , Thermoplastic , Ethylene Methyl Acrylate , Ethylene-Methyl Acrylate Copolymer, Coating Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Ethylene-Methyl Acrylate Copolymer, Coating Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Coating Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.928 - 0.942 g/cc
0.0335 - 0.0340 lb/in³
Average value: 0.935 g/cc Grade Count:9
Viscosity 500000 - 900000 cP

@Temperature 190 - 190 °C
500000 - 900000 cP

@Temperature 374 - 374 °F
Average value: 700000 cP Grade Count:3
500000 - 900000 cP

@Shear Rate 50.0 - 50.0 1/s
500000 - 900000 cP

@Shear Rate 50.0 - 50.0 1/s
Average value: 700000 cP Grade Count:3
Environmental Stress Crack Resistance >= 360 hour

@Temperature 50.0 - 50.0 °C
>= 360 hour

@Temperature 122 - 122 °F
Average value: 360 hour Grade Count:1
Melt Flow 2.00 - 13.5 g/10 min
2.00 - 13.5 g/10 min
Average value: 8.07 g/10 min Grade Count:12
Mechanical Properties Metric English Comments
Seal Strength 1300 - 2800 g/25 mm
1300 - 2800 g/in
Average value: 1960 g/25 mm Grade Count:5
Hot Tack Strength 500 - 2000 g/25 mm
500 - 2000 g/in
Average value: 1030 g/25 mm Grade Count:8
Thermal Properties Metric English Comments
Melting Point 60.0 - 109 °C
140 - 228 °F
Average value: 87.4 °C Grade Count:12
Vicat Softening Point 48.0 - 90.0 °C
118 - 194 °F
Average value: 74.4 °C Grade Count:12
Processing Properties Metric English Comments
Processing Temperature 154 - 315 °C
309 - 599 °F
Average value: 238 °C Grade Count:4
Nozzle Temperature 230 - 305 °C
446 - 581 °F
Average value: 279 °C Grade Count:10
Melt Temperature 220 - 315 °C
428 - 599 °F
Average value: 278 °C Grade Count:8