Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
ExxonMobil LL 6235 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
ExxonMobil LL 6235.19 Injection Molding Resin
(discontinued **) LL 6235 is a narrow molecular weight butene copolymer designed for applications that require easy processability in thin walled parts. This resin offers outstanding toughness and tear resistance in .. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **) LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
ExxonMobil LD 136.MV Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
ExxonMobil LD 136.NI Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
I. Stern 913 High Impact Polystyrene Extrusion Grade Features:Good processing characteristicsExcellent toughness and environmental stress crackingApplicationsThermoformed containers and lids for food packagingCustom extruded sheetInformation provided .. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
Teknor Apex Sinvicomp SRP 5902 Polyvinyl Chloride, Rigid Availability: Asia Pacific Features: High Gloss; High Impact Resistance Uses: Conduit; Piping; Profiles Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
Lubrizol ESTANE® 5707 Ester Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility and superior abrasion and cut resistance. It is processed by means of solution coating, extrusion and melt coating.Uses: S.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
Total PSI 625 Polystyrene Polystyrene 625 is a medium impact polystyrene with balanced physical properties. Thin walled parts with complex runners and gates, run fast and consistently with the easy flow 625. The natural whi.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
ExxonMobil LL 6100.17 Injection Molding Resin Product Description: LL 6100 is a narrow molecular weight butane copolymer designed for applications that require easy processability. This resin offers outstanding toughness and tear resistance in .. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ASA S140 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ASA S150 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | 0.125 inch, 1 Kg; ASTM D1525 |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | ASTM D1525 |
Dow DNDA-8335 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8335 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow Primacor® 4311 Ethylene Acrylic Acid (EAA) PRIMACOR® 4311 polymer containing 3% comonomer 3 is an extrusion/ coextrusion coating and laminating for flexible packaging applications. It is designed to provide excellent adhesion to metallic, p.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow SE SLR-4400 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4400 is manufactured by anionic solution polymerization using lithium initiator. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and non-stai.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow SE SLR-4601 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4601 is manufactured by anionic solution polymerization using lithium initiator. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and chemical.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow SE SLR-4610 H Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4610 H is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium sty.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow SE SLR-4610 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4610 is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of aromatic oil in relation to solid rubber. It is a product with medium styre.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow SE SLR-4630 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4630 is manufactured by anionic solution polymerization using lithium initiator and is extended with 37.5 parts of TDAE oil in relation to solid rubber. It is a product with medium styrene a.. |
|||
Vicat Softening Point | 92.2 °C | 198 °F | |
Dow SE SLR-6410 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-6410 is manufactured by anionic solution polymerization using lithium initiator and is extended with 50 parts of aromatic oil in relation to solid rubber. It is a product with medium styrene.. |