Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Crystallization Temperature = 0.000 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature <= 0.000 °C
<= 32.0 °F
Solvay MIRACARE® 2MCA Surfactant
Description: An optimum blend of anionic and amphoteric surfactants to provide a base concentrate having excellent foaming properties and low irritancy.Chemical Name: AMPHOTERIC/ANIONIC SURFACTANT B..
Copyright © lookpolymers.com All Rights Reserved