Thermal Properties | Metric | English | Comments |
---|---|---|---|
Crystallization Temperature | 116 °C | 241 °F | ASTM D3418 |
ExxonMobil HD 6908.18 Injection Molding Resin
(discontinued **) HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif.. |
|||
Crystallization Temperature | 116 °C | 241 °F | Equate Test Method |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
Crystallization Temperature | 116 °C | 241 °F | Dow Method (DSC) |
Dow DMDA-8940 NT 7 High Density Polyethylene Resin DOW DMDA-8940 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info.. |
|||
Crystallization Temperature | 116 °C | 241 °F | Dow Method (DSC) |
Dow DMDA-8965 NT 7 High Density Polyethylene Resin DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Crystallization Temperature | 116 °C | 241 °F | Dow Method (DSC) |
Dow DMDA-8980 NT 7 High Density Polyethylene Resin DOW DMDA-8980 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Crystallization Temperature | 116 - 122 °C | 241 - 252 °F | |
Addcomp PRIEX® Ionomer 42101 PP homopolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |
|||
Crystallization Temperature | 116 - 122 °C | 241 - 252 °F | |
Addcomp PRIEX® Ionomer 40101 PP homopolymer Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t.. |