Polymer Property : Crystallization Temperature = 241 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 116 °C
241 °F
ASTM D3418
ExxonMobil HD 6908.18 Injection Molding Resin  (discontinued **)
HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif..
Crystallization Temperature 116 °C
241 °F
Equate Test Method
Equate EMDA-6147 HDPE Blow Molding Resin
EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density..
Crystallization Temperature 116 °C
241 °F
Dow Method (DSC)
Dow DMDA-8940 NT 7 High Density Polyethylene Resin
DOW DMDA-8940 NT 7 is produced using UNIPOL™ process technology. It is intended for use in a broad range of injection molding applications such as housewares, toys, food containers and pails. Info..
Crystallization Temperature 116 °C
241 °F
Dow Method (DSC)
Dow DMDA-8965 NT 7 High Density Polyethylene Resin
DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow
Crystallization Temperature 116 °C
241 °F
Dow Method (DSC)
Dow DMDA-8980 NT 7 High Density Polyethylene Resin
DOW DMDA-8980 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow
Crystallization Temperature 116 - 122 °C
241 - 252 °F
Addcomp PRIEX® Ionomer 42101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..
Crystallization Temperature 116 - 122 °C
241 - 252 °F
Addcomp PRIEX® Ionomer 40101 PP homopolymer
Ionomers will be used toStrengthen rigidity and hardness while maintaining impact resistance in polyolefinsMaintain adhesion even under contaminated conditions especially in fatty substratesReduce t..