Polymer Property : Crystallization Temperature = 125 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 125 - 131 °C
257 - 268 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Crystallization Temperature 125 - 130 °C
257 - 266 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 32008 Polyvinylidene Fluoride (PVDF)
Solef® 32008 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Crystallization Temperature 125 °C
257 °F
Dow Method (DSC)
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)
Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri..
Crystallization Temperature >= 125 °C
>= 257 °F
Addcomp ADD-VANCE® NU 489 Nucleation masterbatch, PP based
Fields of application: Extruded and injection molded articles made from PP resins.Examples: Extruded PP sheets, films, tapes and blow molded and injection molded articles, such as garden furniture, ..
Crystallization Temperature 125 - 131 °C
257 - 268 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.