Polymer Property : Crystallization Temperature = 268 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 125 - 131 °C
257 - 268 °F
Peak; ASTM D3418
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Features: Copolymer; Good Flexibility; Low ViscosityUses: Wire & Cable ApplicationsAdditional ..
Crystallization Temperature 125 - 131 °C
257 - 268 °F
Peak, DSC; ASTM D3418
Solvay Specialty Polymers Solef® 31508 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 31508 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.Information provided by Solvay Specialty Polymers.