Polymer Property : Crystallization Temperature = 163 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Crystallization Temperature 73.0 °C
163 °F
ExxonMobil Method
ExxonMobil EXACT™ 3128 Plastomer for Blown Film Applications
Product Description: Exact 3128 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It is designed fro both monolayer and multilayer coextruded ..