Thermal Properties Metric English Comments
Crystallization Temperature <= 170 °C
<= 338 °F
ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin
Product Description: Polybilt 101 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 10..