ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name Polybilt™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Polybilt™ Bitumen Modifier 101 Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Polybilt 101 is compatible with a large variety of bitumens. For optimum results are preliminary study is recommended to determine the base bitumen grade and optimum Polybilt 101 content to achieve the desired end-use properties.Boots binder softening point and decreases penetration.Gives modified blends with excellent storage stability and handling characteristics.Particularly recommended for easy mixing in less compatible bitumen.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabilizer: NoApplications: Bitumen modifierInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ExxonMobil method
Viscosity 3100 cP

@Temperature 190 °C
3100 cP

@Temperature 374 °F
ASTM D3236
Vinyl Acetate Content 14 %
14 %
ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point <= 201 °C
<= 394 °F
Peak Melting Point; ExxonMobil method
Crystallization Temperature <= 170 °C
<= 338 °F
Vicat Softening Point 47.8 °C
118 °F
ASTM D1525
Descriptive Properties Value Comments
Blending Temperature 160-170°C